木塑压纹机一旦出现乳化现象,就会有两种现象出现,第一,液压油发白,正常液压油呈现淡黄色,如果出现乳白色活白色的话,我们要怀疑液压有已经出现乳化现象,同时木塑压纹机会出现增压速度突然变慢,还有就是木塑压纹机压力打不上,这两种现象如果同时出现的话,肯定是液压油乳化了 Once emulsification occurs in the wood plastic embossing machine, there will be two kinds of phenomena. First, the hydraulic oil will turn white, and the normal hydraulic oil will turn light yellow. If there is milky white and active white, we should suspect that the hydraulic pressure has already appeared emulsification. At the same time, the pressure increasing speed of the wood plastic embossing machine will suddenly slow down, and the pressure of the wood plastic embossing machine will not be able to hit, if the two phenomena are the same When it appears, the hydraulic oil must be emulsified 木塑压纹机液压油“乳化‘现象的处理办法 很多企业发现乳化时候一般都是直接更换液压油,还有一个办法就是”熬油"熬油主要操作就是将液压油置于一个大油桶内,在油桶下面加热,可以采用电加热或者直接点火燃烧,一旦油温接近一百度的时候,液压油就会冒泡,同时会发出吱吱的响声,一旦液压油里面含有水分家问世就会发出吱吱响声,如果加温一段时间声音就会越来越小,直到没有声音的时候,说明液压油里面已经不再含有水分了。 How to deal with the phenomenon of "emulsification" of hydraulic oil in wood plastic embossing machine when many enterprises find emulsification, they usually change the hydraulic oil directly. Another way is to boil the oil. The main operation of boiling the oil is to put the hydraulic oil in a large oil barrel and heat it under the oil barrel. It can be electrically heated or directly ignited. Once the oil temperature is close to 100 degrees, the hydraulic oil will Bubbling, at the same time, it will make a squeaking sound. Once the hydraulic oil contains water, it will make a squeaking sound. If it is heated for a period of time, the sound will become smaller and smaller. Until there is no sound, it means that there is no water in the hydraulic oil. |
上一页 有效防止压纹后木纹反弹,确保压纹效果长久稳定 |
下一页 家具压纹机工作原理及特性 |
Copyright © 技术支持:遨游网络